Grade 35SPb20
Corresponding Standard ISO 683-18-2014
Bright steel products
Classification Carbon Steel
35SPb20 Chemical Element Composition Content (%)
Component C Si Mn P S Pb
Minimum Value 0.32 - 0.7 - 0.15 0.15
Maximum Value 0.39 0.4 1.1 0.06 0.25 0.35
35SPb20 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
5≤t≤10 Cold drawn (+C) 640~880 ≥480 ≥6
10<t≤16 Cold drawn (+C) 590~830 ≥400 ≥7
16<t≤40 Cold drawn (+C) 560~800 ≥360 ≥8
40<t≤63 Cold drawn (+C) 530~760 ≥340 ≥9
63<t≤100 Cold drawn (+C) 510~680 ≥300 ≥9
16<t≤40 As-rolled + peeled (+SH) 520~680 ≤198
40<t≤63 As-rolled + peeled (+SH) 520~670 ≤196
63<t≤100 As-rolled + peeled (+SH) 500~650 ≤190
5≤t≤16 Quenched and tempered and peeled (+QT+SH) 630~780 ≥430
16<t≤40 Quenched and tempered and peeled (+QT+SH) 600~750 ≥380 ≥16
40<t≤100 Quenched and tempered and peeled (+QT+SH) 550~700 ≥320 ≥17
5≤t≤10 Quenched and tempered +Cold drawn (+QT+C) 700~900 ≥490 ≥9
10<t≤16 Quenched and tempered +Cold drawn (+QT+C) 700~900 ≥490 ≥11
16<t≤40 Quenched and tempered +Cold drawn (+QT+C) 650~850 ≥455 ≥12
40<t≤63 Quenched and tempered +Cold drawn (+QT+C) 570~770 ≥400 ≥13
63<t≤100 Quenched and tempered +Cold drawn (+QT+C) 550~750 ≥385 ≥14
Approximate Comparison Table
International Organization for Standardization European Standard
ISO EN Numerical Grade
35SPb20 35SPb20 1.0756

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!