Grade 46SiCrMo6
Germany W-Nr. 1.8062
Corresponding Standard DIN EN 10089-2003
Hot-Rolled Steels for Quenched and Tempered Springs Technical Delivery Conditions
Classification Spring Steel
Properties Strength Elasticity Fatigue Resistance Quench Hardness
46SiCrMo6 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo More
Minimum Value 0.42 1.3 0.5 - - 0.5 0.2 Cu+10Sn ±0.60
Maximum Value 0.5 1.7 0.8 0.025 0.025 0.8 0.3
46SiCrMo6 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bar, rod Quenching and Tempering (+QT) 1550~1850 ≥1400 ≥6 ≥35 - ≥10
Bar, rod Cold Shearing Treatment (+S) - - - - ≤280 -
Bar, rod Softening Annealing (+A) - - - ≤248 -
Bar, rod Spheroidizing Annealing (+AC) - - - - ≤230 -
46SiCrMo6 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!