Grade X10CrAlSi7
Germany W-Nr. 1.4713
Corresponding Standard DIN EN 10095-2018
Heat resisting steels and nickel alloys
Classification Ferritic Stainless Steel
Properties Corrosion Resistance
X10CrAlSi7 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Al
Minimum Value - 0.5 - - - 6 0.5
Maximum Value 0.12 1 1 0.04 0.15 8 1
X10CrAlSi7 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Flat steel; 3 ≤ t ≤ 12 Annealing (+A) 420~620 ≥220 long.
≥20
≤192
Flat steel; 3 ≤ t ≤ 12 Annealing (+A) 420~620 ≤220 tr.
≥15
≤192
Flat Steel; t<3 Annealing (+A) 420~620 ≥220 - ≤192
Flat steel; t ≤ 12 Annealing (+A) 420~620 ≥220 Long Products
≥20
≤192
Approximate Comparison Table Ferritic Heat-Resistant Steel
Germany France European Standard Russia
DIN EN/DIN NF EN/NF EN Numerical Grade GOST
X10CrAlSi7 Z8CA7 X10CrAlSi7 1.4713 15KH6SYU
X10CrAlSi7 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!