Grade X10CrAlSi25
Germany W-Nr. 1.4762
Corresponding Standard DIN EN 10095-2018
Heat resisting steels and nickel alloys
Classification Ferritic Stainless Steel
Properties Corrosion Resistance
Density 7.7 g/cm3
X10CrAlSi25 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Al
Minimum Value - 0.7 - - - 23 1.2
Maximum Value 0.12 1.4 1 0.04 0.015 26 1.7
X10CrAlSi25 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Bar; t≤25 Annealing (+A) 520~720 ≥280 ≥10 ≤223
Approximate Comparison Table Heat-Resistant Stainless Steel
Germany France European Standard
DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
X10CrAl 24
X10CrAlSi 25
1.4762
1.4762
Z10CAS 24 X10CrAlSi 25 1.4762

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!