Grade X18CrN 28
Germany W-Nr. 1.4749
Corresponding Standard DIN EN 10095-2018
Heat resisting steels and nickel alloys
Classification Ferritic Stainless Steel
Properties Corrosion Resistance
Density 7.7 g/cm3
X18CrN 28 Chemical Element Composition Content (%)
Component C Si Mn P S Cr N
Minimum Value 0.15 - - - - 26 0.15
Maximum Value 0.2 1 1 0.04 0.015 29 0.25
X18CrN 28 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Coil bars, profiles; t≤25 Annealing (+A) 500~700 ≥280 ≥15 ≤212
X18CrN28 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!