Grade X15CrNiSi20-12
Germany W-Nr. 1.4828
Corresponding Standard DIN EN 10095-2018
Heat resisting steels and nickel alloys
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X15CrNiSi20-12 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - 1.5 - - - 19 11 -
Maximum Value 0.2 2.5 2 0.045 0.015 21 13 0.11
X15CrNiSi20-12 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Flat steel; t≤75 Solid Solution Treatment (+AT) 550~750 ≥230 Long Products
≥30
≤223
Flat steel; 0.5≤t<3 Solid Solution Treatment (+AT) 550~750 ≥230 long. tr.
≥28
≤223
Flat steel; 3≤t≤75 Solid Solution Treatment (+AT) 550~750 ≥230 long. tr.
≥30
≤223
1 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States Germany France European Standard Russia United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST BS EN/BS
16Cr23Ni13
(2Cr23Ni13)
S30920 SUH 309 SUH 309 STR 309 309 S30900 X15CrNiSi 20-12 1.4828 Z15CNS 20-12 X15CrNiSi 20-12 1.4828 20Х20Н14С2 309S24
2 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Japan United States Germany France European Standard Russia United Kingdom
GB JIS ASTM DIN EN/DIN NF EN/NF EN Numerical Grade GOST BS EN/BS
1Cr20Ni14Si2 SUH309 309 X15CrNiSi20-12 Z17CNS20-12 X15CrNiSi20-12 1.4828 20KH20N14S2 309S24

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!