Grade X6NiCrSiNCe 35-25
Germany W-Nr. 1.4854
Corresponding Standard DIN EN 10095-2018
Heat resisting steels and nickel alloys
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Density 7.9 g/cm3
X6NiCrSiNCe 35-25 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N Ce
Minimum Value 0.04 1.2 - - - 24 34 0.12 0.03
Maximum Value 0.08 2 2 0.04 0.015 26 36 0.2 0.08
X6NiCrSiNCe 35-25 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Coil bars, profiles; t≤25 Solid Solution Treatment (+AT) 650~850 ≥300 Long Products
≥40
≤210
Coil, Profile; 0.5≤t<3 Solid Solution Treatment (+AT) 650~850 ≥300 long. tr.
≥40
≤210
Coil, Profile; t≥3 Solid Solution Treatment (+AT) 650~850 ≥300 long. tr.
≥40
≤210