Grade 38CrCoWV18-17-17
Germany W-Nr. 1.2661
Corresponding Standard DIN EN ISO 4957-2018
Tool steels
Classification Alloy Steel
Density 8 g/cm3
38CrCoWV18-17-17 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo W V Co
Minimum Value 0.35 0.15 0.2 - - 4 0.3 3.8 1.7 4
Maximum Value 0.45 0.5 0.5 0.03 0.02 4.7 0.5 4.5 2.1 4.5
• Elements not quoted in this table shall not be intentionally added to the steel without the agreement of the purchaser, other than for the purpose of finishing the heat . All reasonable precautions shall be taken to prevent the addition from scrap or other material used in the manufacture, of such elements which affect the hardenability, mechanical properties and applicability.
38CrCoWV18-17-17 Mechanical Properties
Hardness
HBW
Soft annealing (+A) ≤260
Quenching and Tempering HRC
≥48
Approximate Comparison Table Hot-Work Tool Steels
Taiwan, China International Organization for Standardization Germany European Standard
CNS ISO DIN EN/DIN W-Nr. EN Numerical Grade
SKD8 38CrCoWV18-17-17 38CrCoWV18-17-17 1.2661 38CrCoWV18-17-17 1.2661
38CrCoWV18-17-17 Corresponding Standards(Same grade name, different standards)