Grade 28CrH
China ISC A20285
Corresponding Standard GB /T 5216-2014
Structural Steels Specified Hardenability Bands
Classification Alloy Steel
28CrH Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu O
Minimum Value 0.24 - 0.6 - - 0.9 - - -
Maximum Value 0.31 0.37 0.9 0.03 0.035 1.2 0.3 0.25 0.002
28CrH Mechanical Properties
Heat Treatment or Condition
Hardness
HBW
Annealing or High-Temperature Tempering ≤217
Approximate Comparison Table Hardenability Guaranteed Structural Steel
China International Organization for Standardization Germany European Standard
GB ISO DIN EN/DIN EN Numerical Grade
28CrH 28Cr4 28Cr4 28Cr4 1.7030