Grade 8MnSi7
Germany W-Nr. 1.5113
Corresponding Standard DIN EN 10263-2-2017
Steel Rod, Bars and Wire for Cold Heading and Cold Extrusion - Part 2: Technical Delivery Conditions for Steels Not Intended for Heat Treatment after Cold Working
Classification Alloy Steel
8MnSi7 Chemical Element Composition Content (%)
Component C Si Mn P S Al *
Minimum Value - 0.9 1.6 - - -
Maximum Value 0.1 1.1 1.8 0.025 0.025 0.02
8MnSi7 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Coil Bar, Steel Bar; 5<d≤10 Hot Rolled or Untreated and Pickled (+U or +U+PE) ≤540 ≥60
Coil, Steel Bar; 10<d≤25 Hot Rolled or Untreated and Pickled (+U or +U+PE) ≤520 ≥60
Steel Bar, Wire; 5<d≤25 Untreated and Cold Drawn (+U+C) ≥800
8MnSi7 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!