Grade 20NiCrMo 7
Germany W-Nr. 1.3576
Corresponding Standard DIN EN ISO 683-17-2015
Heat-Treated Steels, Alloy Steels and Free-Cutting Steels - Part 17: Ball and Roller Bearing Steels
Classification Alloy Steel
Properties Quench Hardness
20NiCrMo 7 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Al O
Minimum Value 0.17 - 0.4 - - 0.35 1.6 - 0.2 - -
Maximum Value 0.23 0.4 0.7 0.025 0.015 0.65 2 0.3 0.3 0.05 0.002
20NiCrMo 7 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Steel billet, bar stock, coil bar Cold Shearing Treatment (+S) ≤255
Bars, coiled bars Softening Annealing (+A) ≤229
Bar stock, coil, wire, ring parts Solution Heat Treatment (+TH) 174~229
Bars, coils, wire rods, pipes, rings Spheroidizing Annealing (+AC) ≤170
Bar, Coil, Pipe, Ring Isothermal Treatment to Ferrite-Perlite Structure and Hardness Range (+FP) 154~207

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!