Grade C56E2
Germany W-Nr. 1.1219
Corresponding Standard DIN EN ISO 683-17-2015
Heat-Treated Steels, Alloy Steels and Free-Cutting Steels - Part 17: Ball and Roller Bearing Steels
Classification Alloy Steel
C56E2 Chemical Element Composition Content (%)
Component C Si Mn P S Cu Al O
Minimum Value 0.52 - 0.6 - - - - -
Maximum Value 0.6 0.4 0.9 0.025 0.015 0.3 0.05 0.002
C56E2 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Steel billet, bar stock, coil bar Cold Shearing Treatment (+S) ≤255
Bars, coiled bars Softening Annealing (+A) ≤229
C56E2 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!