Grade 12Ni14
Corresponding Standard ISO 9328-4-2018
Nickel-Alloy Steels with Specified Low Temperature Properties
Classification Alloy Steel
12Ni14 Chemical Element Composition Content (%)
Component C Si Mn P S Ni V More
Minimum Value - - 0.3 - - 3.25 - Cr+Cu+Mo≤0.50
Maximum Value 0.15 0.35 0.8 0.02 0.005 3.75 0.05
12Ni14 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
t≤30 Normalizing (+N) or Normalizing and Tempering (+NT) or Quenching and Tempering (+QT) 490~640 ≥355 ≥22
30<t≤50 Normalizing (+N) or Normalizing and Tempering (+NT) or Quenching and Tempering (+QT) 490~640 ≥345 ≥22
50<t≤80 Normalizing (+N) or Normalizing and Tempering (+NT) or Quenching and Tempering (+QT) 490~640 ≥335 ≥22
1 Approximate Comparison Table Pressure-Bearing Flat Steel
International Organization for Standardization European Standard
ISO Numerical Grade
12Ni14 1.5637
2 Approximate Comparison Table Pressure-Bearing Flat Steel
China Japan United States International Organization for Standardization European Standard
GB JIS ASTM ISO EN
08Ni3DR
GB/T 713.4-2023
SL3N255
SL3N275
SL3N440
JIS G 3127-2021
3.5%Ni D级
3.5%Ni E级
3.5%Ni F级
ASTM A203/A203M-17
12Ni14
ISO 9328-4-2018
12Ni14
EN 10028-4-2017
12Ni14 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!