Grade NiCr8020
Germany W-Nr. 2.4869
Corresponding Standard DIN 17750-2002
Wrought nickel and nickel alloy sheet,plate and strip Requirements and testing
Classification Alloy Steel
Properties Corrosion Resistance
Density 8.3 g/cm3
NiCr8020 Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Ni Cu Co Al
Minimum Value - - 0.5 - - - 19 75 - - -
Maximum Value 1 0.15 2 1 0.02 0.015 21 - 0.5 1.5 0.3
NiCr8020 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Strip steel; 0.2<t≤2.5 Solution treatment (F60) ≥600 ≥220 ≥25 ≤230
Thin and thick plates; 1<t≤25 Solution treatment (F60) ≥600 ≥220 ≥25 ≤230
Approximate Comparison Table High-Resistance Electric Heating Alloy
China Japan United States Germany France Russia United Kingdom
GB JIS ASTM DIN EN/DIN NF EN/NF GOST BS EN/BS
Cr20Ni80 NCHW-1
NCHR-1
80Ni20Cr NiCr8020 RNC 苏佩尔安非 Х20Н80-Н 勃来捷尔
阿洛依C.S
NiCr8020 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!