Grade NiCr20CuMo
Germany W-Nr. 2.4660
Corresponding Standard DIN 17750-2002
Wrought nickel and nickel alloy sheet,plate and strip Requirements and testing
Classification Alloy Steel
Properties Corrosion Resistance
Density 8.1 g/cm3
NiCr20CuMo Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Co More
Minimum Value - - - - - 19 32 3 2 - Fe:余量;Nb+Ta:8C~1
Maximum Value 0.07 1 2 0.025 0.015 21 38 4 3 1.5
NiCr20CuMo Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Strip steel; 0.2<t≤2.5 Softening Annealing (F55) ≥550 ≥240 ≥40 ≤220
Thin and thick plates; 1<t≤25 Softening Annealing (F55) ≥550 ≥240 ≥40 ≤220
Approximate Comparison Table Corrosion-Resistant Alloy
China United States Germany
GB ISC Commercial Grade UNS DIN EN/DIN W-Nr.
NS 1403
(NS143)
(0Cr20Ni35Mo3Cu4Nb)
H 08020
H 01403
Alloy 20cb3
Carpenter 20Cb3
N 08020 NiCr20CuMo 2.4660
NiCr20CuMo Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!