Grade 34CrS4
Corresponding Standard ISO 683-2-2016
Alloy steels for quenching and tempering
Classification Alloy Steel
34CrS4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu
Minimum Value 0.3 0.1 0.6 - 0.02 0.9 -
Maximum Value 0.37 0.4 0.9 0.025 0.04 1.2 0.4
34CrS4 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bar, flat material, forging; d≤16 or t≤8 Quenching and Tempering 900~1100 ≥700 ≥12 ≥35
Bar, flat material, forging; 16<d≤40 or 8<t≤20 Quenching and Tempering 800~950 ≥590 ≥14 ≥40 ≥40
Bar, flat material, forging; 40<d≤100 or 20<t≤60 Quenching and Tempering 700~850 ≥460 ≥15 ≥45 ≥40
Bars, semi-finished products Processed to improve shearability (+S) ≤255
Bars, flat products, forgings, semi-finished products, rebar Soft Annealing (+A) ≤223
Approximate Comparison Table
International Organization for Standardization Germany France European Standard
ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
34CrS4 34CrS4 1.7037 32C4u 34CrS4 1.7037

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!