Grade 34CrNiMo6
Corresponding Standard ISO 683-2-2016
Alloy Steels for Quenching and Tempering
Classification Alloy Steel
34CrNiMo6 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.3 0.1 0.5 - - 1.3 1.3 - 0.15
Maximum Value 0.38 0.4 0.8 0.025 0.035 1.7 1.7 0.4 0.3
34CrNiMo6 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bar, flat material, forging; d≤16 or t≤8 Quenching and Tempering 1200~1400 ≥1000 ≥9 ≥40
Bar, flat material, forging; 16<d≤40 or 8<t≤20 Quenching and Tempering 1100~1300 ≥900 ≥10 ≥45 ≥45
Bar, flat material, forging; 40<d≤100 or 20<t≤60 Quenching and Tempering 1000~1200 ≥800 ≥11 ≥50 ≥45
Bars, flat products, forgings; 100<d≤160 or 60<t≤100 Quenching and Tempering 900~1100 ≥700 ≥12 ≥55 ≥45
Bars, Flats, Forgings; 160<d≤250 or 100<t≤160 Quenching and Tempering 800~950 ≥600 ≥13 ≥55 ≥45
Bars, flat products, forgings, semi-finished products, rebar Soft Annealing (+A) ≤248
1 Approximate Comparison Table Structural Alloy Steel
China International Organization for Standardization European Standard
GB ISO EN Numerical Grade
34Cr2Ni2Mo 34CrNiMo6 34CrNiMo6 1.6582
2 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization European Standard
ISO EN Numerical Grade
34CrNiMo6 34CrNiMo6 1.6582

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!