Grade 33CrMoV12-9
Corresponding Standard ISO 683-5-2017
Nitriding steels
Classification Alloy Steel
33CrMoV12-9 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo V
Minimum Value 0.29 - 0.4 - - 2.8 0.7 0.15
Maximum Value 0.36 0.4 0.7 0.025 0.035 3.3 1 0.25
33CrMoV12-9 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
16≤d≤40, 8≤t≤20 Quenching and Tempering 1150~1350 ≥950 ≥11 ≥30
40≤d≤100, 20≤t≤60 Quenching and Tempering 1050~1250 ≥850 ≥12 ≥35
100≤d≤160, 60≤t≤100 Quenching and Tempering 950~1150 ≥750 ≥12 ≥40
160≤d≤250, 100≤t≤160 Quenching and Tempering 900~1100 ≥700 ≥13 ≥45
Approximate Comparison Table Nitriding Steels
International Organization for Standardization European Standard
ISO EN Numerical Grade
33CrMoV12-9 33CrMoV12-9 1.8522