Grade C75S
Germany W-Nr. 1.1248
Corresponding Standard DIN EN 10132-4-2000(+AC:2002)
Cold-rolled narrow steel strip for heat treatment-Technical delivery conditions Part 4: Spring steels and other applications (includes Corrigendum AC:2002)
Classification Spring Steel
C75S Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.7 0.15 0.6 - - - - -
Maximum Value 0.8 0.35 0.9 0.025 0.025 0.4 0.4 0.1
C75S Mechanical Properties
thickness
t
mm
Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
0.3≤t≤3 C75S A/LC Annealing (+A) or Annealing and Flattening (+LC) ≤640 ≤510 ≥15 HV
≤200
0.3≤t≤3 C75S CR Cold Rolled (+CR) ≤1170 ≤320
0.3≤t≤3 C75S QT Tempering (+QT) 1200~1900 370~580
New and Old Grade Replacement List
Corresponding Standard Grade
DIN 17222-1979
Grade
Germany W-Nr.
Old Grade
DIN EN 10132-4-2000(+AC:2002)
Grade
Germany W-Nr.
Approximate Comparison Table Spring Steel
United States Germany France European Standard Russia Sweden United Kingdom
AISI UNS DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS14 BS EN/BS
1078 G10780 Ck75 1.1248 C75RR C75S 1.1248 75A 1774 CS80
C75S Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!