Grade C67S
Germany W-Nr. 1.1231
Corresponding Standard DIN EN 10132-4-2000(+AC:2002)
Cold-rolled narrow steel strip for heat treatment-Technical delivery conditions Part 4: Spring steels and other applications (includes Corrigendum AC:2002)
Classification Spring Steel
Properties Strength Elasticity
C67S Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.65 0.15 0.6 - - - - -
Maximum Value 0.73 0.35 0.9 0.025 0.025 0.4 0.4 0.1
C67S Mechanical Properties
thickness
t
mm
Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
0.3≤t≤3 C67S A/LC Annealing (+A) or Annealing and Flattening (+LC) ≤600 ≤510 ≥16 HV
≤200
0.3≤t≤3 C67S CR Cold rolled (+CR) ≤1140 HV
≤315
C67S QT Quenching and Tempering (+QT) 1200~1900 HV
370~580
New and Old Grade Replacement List
Corresponding Standard Grade
DIN 17222-1979
Grade
Germany W-Nr.
DIN EN 10132-4-2000(+AC:2002)
Grade
Germany W-Nr.
1 Approximate Comparison Table High-Quality Carbon Structural Steel
China United States International Organization for Standardization Germany France Russia Sweden United Kingdom
GB ISC ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST SS BS EN/BS
65 U20652 1065 G10650 SL
SM
Ck67 1.1231 XC65 65 1770 060A67
2 Approximate Comparison Table Spring Steel
China Japan United States International Organization for Standardization Germany France Russia Sweden United Kingdom
GB ISC JIS AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST SS14 BS EN/BS
65 U20652 SUP2 1065 G10650 Type DC Ck67 1.1231 XC65 65 1770 060A67
C67S Corresponding Standards(Same grade name, different standards)