Grade 125Cr2
Germany W-Nr. 1.2002
Corresponding Standard DIN EN 10132-4-2000(+AC:2002)
Cold-Rolled Narrow Steel Strip for Heat Treatment-Technical Delivery Conditions Part 4: Spring Steels and Other Applications (Includes Corrigendum AC:2002)
Classification Spring Steel
125Cr2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 1.2 0.15 0.25 - - 0.4 - -
Maximum Value 1.3 0.35 0.4 0.025 0.025 0.6 0.4 0.1
125Cr2 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
0.3≤t≤3 Annealing (+A) or Annealing and Flattening (+LC) ≤750 ≤590 ≥11 HV
≤235
0.3≤t≤3 Tempering (+QT) 1300~2100 405~630
125Cr2 Corresponding Standards(Same grade name, different standards)