Grade 10CrMo9-10
European Standard Steel Grade 1.7380
Corresponding Standard EN 10028-2-2009
Flat products made of steels for pressure purposes Part 2 Non-alloy and alloy steels with specified elevated temperature properties
Classification Alloy Steel
10CrMo9-10 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu Mo N
Minimum Value 0.08 - 0.4 - - 2 - 0.9 -
Maximum Value 0.14 0.5 0.8 0.02 0.01 2.5 0.3 1.1 0.012
10CrMo9-10 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t≤16 Normalizing and Tempering (+NT) 480~630 ≥310 ≥18 *
≥31
16<t≤40 Normalizing and Tempering (+NT) 480~630 ≥300 ≥18 ≥31
40<t≤60 Normalizing and Tempering (+NT) 480~630 ≥290 ≥18 ≥31
60<t≤100 Normalizing and Tempering (+NT) or Quenching and Tempering (+QT) 470~620 ≥280 ≥17 ≥27
100<t≤150 Quenching and Tempering (+QT) 460~610 ≥260 ≥17 ≥27
150<t≤250 Quenching and Tempering (+QT) 450~600 ≥250 ≥17 ≥27
1 Approximate Comparison Table Pressure-Bearing Flat Steel
International Organization for Standardization European Standard
ISO EN Numerical Grade
10CrMo 9-10 10CrMo 9-10 1.7380
2 Approximate Comparison Table Structural Alloy Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
12CrMo SCMV4 A387Gr.22
Gr.P22
F34
P34
TS34
10CrMo9-10 10CD9-10
12CD9-10
10CrMo9-10 1.7380 10KH2M 2218 622
622Gr.31
3 Approximate Comparison Table Seamless Steel Tubes and Pipes for High Pressure Boiler
China United States European Standard
GB ISC ASTM/AISI EN
12Cr2MoG A30128 SA-213 T22
SA-335 P22
10CrMo9-10

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!