Grade X39Cr13
European Standard Steel Grade 1.4031
Corresponding Standard EN 10088-2-2005
Classification Martensitic Stainless Steel
Properties Corrosion Resistance
X39Cr13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr
Minimum Value 0.36 - - - - 12.5
Maximum Value 0.42 1 1 0.04 0.015 14.5
X39Cr13 Mechanical Properties
thickness
t
mm
Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
t≤3 1.4031 C+QT Cold rolled steel strip (C) and tempered (+QT) HV
480~580
t≤8 1.4031 C+A Cold rolled steel strip (C) and annealed (+A) ≤760 ≥12 ≤240
t≤13.5 1.4031 H+A Hot rolled steel strip (H) and annealing (+A) ≤760 ≥12 ≤240
1 Approximate Comparison Table Martensitic Stainless Steel
China United States International Organization for Standardization Germany France European Standard Russia
GB ISC UNS ISO Numerical Grade DIN EN/DIN NF EN/NF EN Numerical Grade GOST
40Cr13
(4Cr13)
S42040 S42000 X39Cr 13
X46Cr13
X52Cr13
4031-420-00-I
4034-420-00-I
4038-420-00-I
X38Cr 13 Z40C 14 X39Cr 13 1.4031
1.4034
(1.4038)
40Х13
2 Approximate Comparison Table Other Stainless Steels
Germany France European Standard Sweden
DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS
X38Cr 13
X39Cr 13
1.4031
1.4031
Z40C14 X39Cr13 1.4031 2340
3 Approximate Comparison Table Martensitic Stainless Steel
China United States Germany France European Standard Russia United Kingdom
GB ASTM DIN EN/DIN NF EN/NF EN Numerical Grade GOST BS EN/BS
4Cr13 Type420 X39Cr13 Z40C13 X39Cr13 1.4031 40KH13 X39Cr13

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!