Grade ZG1Cr18Mn8Ni4N
China ISC 309
Corresponding Standard GB 2100-1980
Technical Conditions for Stainless Acid-Resistant Steel Castings
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
ZG1Cr18Mn8Ni4N Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - 7.5 - - 17 3.5 0.15
Maximum Value 0.1 1.5 10 0.06 0.03 19 5.5 0.25
ZG1Cr18Mn8Ni4N Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Quenching 1100~1150°C, Water Cooling ≤588 ≤245 ≤40 ≤50

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!