Grade 24CrMo13-6
European Standard Steel Grade 1.8516
Corresponding Standard EN 10085-2001
Nitriding Steels. Technical Delivery Conditions
Classification Alloy Steel
24CrMo13-6 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo
Minimum Value 0.2 - 0.4 - - 3 0.5
Maximum Value 0.27 0.4 0.7 0.025 0.035 3.5 0.7
24CrMo13-6 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bars, flat products, forgings; 16≤d≤40 Quenching and Tempering (+QT) 1000~1200 ≥800 ≥10 - ≥25
Bars, flat products, forgings; 40<d≤100 Quenching and Tempering (+QT) 950~1150 ≥750 ≥11 - ≥30
Bars, flat products, forgings; 100<d≤160 Quenching and Tempering (+QT) 900~1100 ≥700 ≥12 - ≥30
Bars, flat products, forgings; 160<d≤250 Quenching and Tempering (+QT) 850~1050 ≥650 ≥13 - ≥30
Bars, rods, flat products, forgings, semifinished products Soft Annealing (+A) - - - ≤248 -
Approximate Comparison Table Nitriding Steels
International Organization for Standardization European Standard
ISO EN Numerical Grade
24CrMo13-6 24CrMo13-6 1.8516
24CrMo13-6 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!