Grade 32CrAlMo7-10
European Standard Steel Grade 1.8505
Corresponding Standard EN 10085-2001
Nitriding Steels. Technical Delivery Conditions
Classification Alloy Steel
32CrAlMo7-10 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo Al
Minimum Value 0.28 - 0.4 - - 1.5 0.2 0.8
Maximum Value 0.35 0.4 0.7 0.025 0.035 1.8 0.4 1.2
32CrAlMo7-10 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bars, flat products, forgings; 16≤d≤40 Quenching and Tempering (+QT) 1030~1230 ≥835 ≥10 - ≥25
Bars, flat products, forgings; 40<d≤100 Quenching and Tempering (+QT) 980~1180 ≥835 ≥10 - ≥25
Bars, flat products, forgings; 100<d≤160 Quenching and Tempering (+QT) 930~1130 ≥735 ≥12 - ≥30
Bars, flat products, forgings; 160<d≤250 Quenching and Tempering (+QT) 880~1080 ≥675 ≥12 - ≥30
Bars, rods, flat products, forgings, semifinished products Soft Annealing (+A) - - - ≤248 -
Approximate Comparison Table Nitriding Steels
International Organization for Standardization European Standard
ISO EN Numerical Grade
32CrAlMo7-10 32CrAlMo7-10 1.8505
32CrAlMo7-10 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!