Grade 33CrMoV12-9
European Standard Steel Grade 1.8522
Corresponding Standard EN 10085-2001
Nitriding Steels. Technical Delivery Conditions
Classification Alloy Steel
33CrMoV12-9 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo V
Minimum Value 0.29 - 0.4 - - 2.8 0.7 0.15
Maximum Value 0.36 0.4 0.7 0.025 0.035 3.3 1 0.25
33CrMoV12-9 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bars, flat products, forgings; 16≤d≤40 Quenching and Tempering (+QT) 1150~1350 ≥950 ≥11 - ≥30
Bars, flat products, forgings; 40<d≤100 Quenching and Tempering (+QT) 1050~1250 ≥850 ≥12 - ≥35
Bars, flat products, forgings; 100<d≤160 Quenching and Tempering (+QT) 950~1150 ≥750 ≥12 - ≥40
Bars, flat products, forgings; 160<d≤250 Quenching and Tempering (+QT) 900~1100 ≥700 ≥13 - ≥45
Bars, rods, flat products, forgings, semifinished products Soft Annealing (+A) - - - ≤248 -
Approximate Comparison Table Nitriding Steels
International Organization for Standardization European Standard
ISO EN Numerical Grade
33CrMoV12-9 33CrMoV12-9 1.8522