Grade C35
European Standard Steel Grade 1.0501
Corresponding Standard EN 10083-2-2006
Steels for quenching and tempering. Part 2:Technical delivery conditions for non alloy steels
Brand/Supplier
-> BAOSTEEL
Classification Carbon Steel
C35 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo More
Minimum Value 0.32 - 0.5 - - - - - Cr+Mo+Ni≤ 0.63
Maximum Value 0.39 0.4 0.8 0.045 0.045 0.4 0.4 0.1
1 Approximate Comparison Table
China Japan International Organization for Standardization European Standard
GB JIS ISO EN Numerical Grade
35 S35C C35 C35 1.0501
2 Approximate Comparison Table
United States International Organization for Standardization Germany France European Standard United Kingdom
ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade BS EN/BS
1035 C35R
C35M2
C35
Cm35
XC38H1u C35R 1.1180 080M36
3 Approximate Comparison Table
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
35 S35C 1035
Gr.1035
C35
C35E4
C35 1.0501 AF55C35
C35
C35 1.0501 35
40
1550 070M36
40HS
4 Approximate Comparison Table
China Japan United States International Organization for Standardization France Russia United Kingdom
GB JIS ASTM/AISI ISO NF EN/NF GOST BS EN/BS
GB/T 699-1999
35
S35C 1035 ISO 630-1:1987
C35
C35E4
C35M2
C35
XC35
35 060A35
5 Approximate Comparison Table
China Japan United States Germany France Russia United Kingdom
GB JIS ASTM/AISI DIN EN/DIN W-Nr. NF EN/NF GOST BS EN/BS
35Mn
(GB/T 699-1999)
SWRCH35K 1037 C35 1.0501 C35 35Г 080A35
080A36
C35

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!