Grade X7CrTi12
1.4720
Corresponding Standard SEW 470(1976)
Heat-resisting rolled and forged steels
Classification Ferritic Stainless Steel
Properties Corrosion Resistance
Density 7.7 g/cm3
X7CrTi12 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ti
Minimum Value - - - - - 10.5 -
Maximum Value 0.08 1 1 0.04 0.03 12.5 1
X7CrTi12 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Steel plate, steel strip, steel pipe, steel bar, forged product, steel wire Annealing 400~600 ≥210 25 ≤179

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!