Grade X10Cr 13
Corresponding Standard EU 95-1979
Heat Resistant Steel: Technical Delivery Conditions
Classification Martensitic Stainless Steel
Properties Corrosion Resistance
Density 7.7 g/cm3
X10Cr 13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr
Minimum Value - - - - - 12
Maximum Value 0.12 1 1 0.04 0.03 14
X10Cr 13 Mechanical Properties
product Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Bar, flat material, forged product, plate, strip, wire Annealing 450~650 ≥250 ≥20 ≤192
X10Cr13 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!