Grade 51CrMnV
China ISC A25513
Corresponding Standard GB /T 1222-2016
Spring steels
Classification Spring Steel
51CrMnV Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu * V
Minimum Value 0.47 0.17 0.7 - - 0.9 - - 0.1
Maximum Value 0.55 0.37 1.1 0.025 0.02 1.2 0.35 0.25 0.25
51CrMnV Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Quenching and Tempering ≥1350 ≥1200 ≥6 ≥30 -
Hot Rolled (WHR) - - - - Negotiated Between Supplier and Buyer
Stress relief annealing (A) - - - - ≤280
Soft annealing (SA) - - - - ≤248

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!