Grade 37Cr4
Corresponding Standard ISO 4954-2018
Steels for cold heading and cold extruding
Classification Alloy Steel
37Cr4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu
Minimum Value 0.34 - 0.6 - - 0.9 -
Maximum Value 0.41 0.3 0.9 0.025 0.025 1.2 0.25
37Cr4 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
5<d≤40 +AC or +AC+PE ≤590 ≥60
2<d≤5 +AC+C+AC ≤580 ≥62
5<d≤40 +AC+C+AC ≤570 ≥62
2<d≤5 +AC+C+AC+LC ≤620 ≥60
5<d≤40 +AC+C+AC+LC ≤610 ≥60
1 Approximate Comparison Table
China International Organization for Standardization European Standard
GB ISO EN Numerical Grade
35Cr 37Cr4 37Cr4 1.7034
2 Approximate Comparison Table structural alloy steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
35Cr SCr435H Gr.5135 37Cr4 37Cr4 1.7034 37Cr4
38C4
37Cr4 1.7034 38KHA
40KH
2245 530A36
530M36
3 Approximate Comparison Table
International Organization for Standardization European Standard
ISO EN Numerical Grade
37Cr4 37Cr4 1.7034

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!