Grade 41CrS4
Corresponding Standard ISO 4954-2018
Steels for cold heading and cold extruding
Classification Alloy Steel
41CrS4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu
Minimum Value 0.38 - 0.6 - 0.02 0.9 -
Maximum Value 0.45 0.3 0.9 0.025 0.04 1.2 0.25
41CrS4 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
5<d≤40 +AC or +AC+PE ≤620 ≥58
2<d≤5 +AC+C+AC ≤610 ≥60
5<d≤40 +AC+C+AC ≤600 ≥60
2<d≤5 +AC+C+AC+LC ≤650 ≥58
5<d≤40 +AC+C+AC+LC ≤640 ≥58
1 Approximate Comparison Table
International Organization for Standardization Germany France European Standard Russia Sweden
ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS
41CrS4 41CrS4 1.7039 42C4u 41CrS4 1.7039 40KH 2245
2 Approximate Comparison Table
International Organization for Standardization European Standard
ISO EN Numerical Grade
41CrS4 41CrS4 1.7039