Grade 25CrMoS4
Corresponding Standard ISO 4954-2018
Steels for cold heading and cold extruding
Classification Alloy Steel
25CrMoS4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu Mo
Minimum Value 0.22 - 0.6 - 0.02 0.9 - 0.15
Maximum Value 0.29 0.3 0.9 0.025 0.04 1.2 0.25 0.3
25CrMoS4 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
5<d≤40 +AC or +AC+PE ≤580 ≥60
2<d≤5 +AC+C+AC ≤570 ≥62
5<d≤40 +AC+C+AC ≤560 ≥62
2<d≤5 +AC+C+AC+LC ≤610 ≥60
5<d≤40 +AC+C+AC+LC ≤600 ≥60
1 Approximate Comparison Table
International Organization for Standardization Germany France European Standard
ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
25CrMoS4 25CrMoS4 1.7213 25CD4u 25CrMoS4 1.7213
2 Approximate Comparison Table
International Organization for Standardization European Standard
ISO EN Numerical Grade
25CrMoS4 25CrMoS4 1.7213