Grade Incoloy alloy 25-6MoHN
USA UNS N08367
Other Names
Brand/Supplier
America ->
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Density 8.06 g/cm3
Incoloy alloy 25-6MoHN Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - - - - 20 23.5 - 6 0.18
Maximum Value 0.03 1 2 0.04 0.03 22 25.5 0.75 7 0.25
Incoloy alloy 25-6MoHN Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Annealing 744 381 48 HRB
90
Approximate Comparison Table Austenitic Stainless Steel
Japan United States International Organization for Standardization European Standard
JIS UNS ISO Numerical Grade Numerical Grade
SUS836L N08367 X2NiCrMoN25-21-7 4478-083-67-U (1.4478)