Grade JFE-HITEN710M
Brand/Supplier
Japan -> JFE Steel
Classification Alloy Steel
Properties Strength Weldability
JFE-HITEN710M Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo V B
Minimum Value - - - - - - 0.3 - - - -
Maximum Value 0.14 0.35 1.2 0.015 0.015 0.7 1.3 0.4 0.5 0.05 0.005
JFE-HITEN710M Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t≤12 Quenching and Tempering 710~840 ≥620 ≥17 -
12<t≤16 Quenching and Tempering 710~840 ≥620 ≥17 -15°C
≥47
16<t≤32 Quenching and Tempering 710~840 ≥620 ≥25 -15°C
≥47
32<t≤50 Quenching and Tempering 710~840 ≥620 ≥25 -20°C
≥47
50<t≤75 Quenching and Tempering 710~840 ≥620 - -30°C
≥47
t>75 Quenching and Tempering 710~840 ≥600 - -30°C
≥47

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!