Grade 50
Other Names
Corresponding Standard GB /T 3078-2019
Quality Structural Steel Cold Drawm Bars
Classification Carbon Steel
50 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Delivery condition Annealing, Bright Annealing, High-Temperature Tempering or Normalizing and Tempering ≤229
Delivery condition Cold Drawing, Cold Drawing and Polishing ≤255
Delivery condition Cold Drawing ≥655 ≥6 ≥30
Delivery condition Annealing ≥560 ≥12 ≥40
1 Approximate Comparison Table High-Quality Carbon Structural Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST SS BS EN/BS
50 U20502 S50C S50C SM50C 1050 G10500 C50E4 C50E
Ck53
1.1210 C50E 50 1674 C50E
080M50
2 Approximate Comparison Table Carbon Structural Steel and Engineering Steel
China Japan International Organization for Standardization
GB JIS ISO
50 S50C C50
3 Approximate Comparison Table Non-Alloy Steel for Quenching and Tempering
China Japan International Organization for Standardization European Standard
GB JIS ISO EN Numerical Grade
50 S50C C50E C50E 1.1206
4 Approximate Comparison Table High-Quality Carbon Structural Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
50 S50C 1049
1050
C50
C50E4
C50
Ck50
XC48H1 C50 1.0540 50 1674 070M50
080M50
5 Approximate Comparison Table High-Quality Carbon Structural Steel
China Japan United States International Organization for Standardization France Russia United Kingdom
GB JIS ASTM/AISI ISO NF EN/NF GOST BS EN/BS
GB/T 699-1999
50
S50C 1049
1050
ISO 630-1:1987
C50
C50E4
C50M2
C50
XC48
50 060A52

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!