Grade 35CrMo
Corresponding Standard GB /T 3078-2019
Quality structural steel cold drawm bars
Classification Alloy Steel
35CrMo Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Delivery condition Annealing, Bright Annealing, High-Temperature Tempering or Normalizing and Tempering ≤241
Delivery condition Cold Drawing, Cold Drawing and Polishing ≤269
1 Approximate Comparison Table structural alloy steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS14 BS EN/BS
35CrMo
35CrMoV
A30352
A31352
SCM435 SCM435
SCM435H
SCM435 4135 G41350 34CrMo4 34CrMo4 1.7220 35CD4 34CrMo4 1.7220 35XM
35ХМФ
2234 708A37
CDS13
2 Approximate Comparison Table structural alloy steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
35CrMo
ZG35CrMo
SCM435H 4135 34CrMo4 34CrMo4 34CD4
35CD4
34CrMo4 1.7220 35KHM
35KHML
2234 708A30
708M32
3 Approximate Comparison Table cast steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
ZG35CrMo
35CrMo
SCM435H 4135 34CrMo4 34CrMo4 34CD4
35CD4
34CrMo4 1.7220 35KHM
35KHML
2234 708A30
708M32

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!