Grade Q275A
China ISC U12752
Other Names
Corresponding Standard GB /T 3274-2017
Hot-Rolled Plates, Sheets and Strips of Carbon Structural Steels and High Strength Low Alloy Structural Sheets
Brand/Supplier
-> BAOSTEEL
Classification Carbon Steel
Properties Weldability
Q275A Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu As N
Minimum Value - - - - - - - - - -
Maximum Value 0.24 0.35 1.5 0.045 0.05 0.3 0.3 0.3 0.08 0.008
Q275A Mechanical Properties
thickness(diameter)
t(d)
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
≤16 410~540 ≥275 ≥22
>16~40 410~540 ≥265 ≥22
>40~60 410~540 ≥255 ≥21
>60~100 410~540 ≥245 ≥20
>100~150 410~540 ≥225 ≥18
>150~200 410~540 ≥215 ≥17
1 Approximate Comparison Table Carbon Structural Steel and Engineering Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France Russia Sweden United Kingdom
GB ISC CNS JIS KS UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST SS BS EN/BS
Q275
(C5)
U12752 SS490 SS490
(SS50)
SS490 K02901 Fe430A S275J2G3
S275J2G4
(St44-3N)
1.0144
1.0145
1.0055
S275J2G3
S275J2G4
Ст5кп-2
Ст5кп
БСт5кп-2
1430 S275J2G3
S275J2G4
(43D)
2 Approximate Comparison Table Carbon Structural Steel and Engineering Steel
China Japan United States International Organization for Standardization European Standard
GB ISC JIS ASTM/AISI ISO EN Numerical Grade
Q275A
(GB/T 700-2006)
U12752 SS490
(JIS G3101:2004)
(JIS G3106:2004)
Gr.70[290]
(ASTM A573/A573M:2000)
E275A
(ISO 630:1995)
S275JR
(EN 10025-2:2004)
1.0044
Q275A Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!