Grade HR760T/ 660Y-MP
Corresponding Standard GMW 3399-2013
Multi-phase and Ultra-high Strength Sheet Steel
Classification Alloy Steel
HR760T/ 660Y-MP Chemical Element Composition Content (%)
Component C Si Mn P S Cu Al More
Minimum Value - - - - - - 0.01 (Ni+Cr+Mo)<1.5*;B:N/A
Maximum Value 0.25 2 2.2 0.05 0.015 0.2 -
Note: Chemical composition based on mass% product (coil or sheet/blank) analysis.
HR760T/ 660Y-MP Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hot Rolling ≥760 660~820 *
≥10

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!