Grade 30CrMnSiA
Corresponding Standard GJB 2150A-2005
Specification for hot-rolled alloy structure steel sheets and plates for avication
Classification Alloy Steel
30CrMnSiA Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo W
Minimum Value 0.28 0.9 0.8 - - 0.8 - - - -
Maximum Value 0.34 1.2 1.1 0.025 0.025 1.1 0.3 0.25 0.13 0.13
30CrMnSiA Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
≤4※ Delivery Condition 540~735 ≥16 ≤229
>4※ Delivery Condition 540~735 ≥19 ≤229
Sample* Quenching or Tempering 880~900°C oil quenching; Tempering 500~560°C oil or water quenching ≥1080 ≥10