Grade EVERHARD-C450LE
Brand/Supplier
Japan -> JFE Steel
Classification Alloy Steel
EVERHARD-C450LE Chemical Element Composition Content (%)
  Component C Si Mn P S Cr Mo Ti B More
适用板厚5~19mm Minimum Value - - - - - - - - - Ceq≤0.5
Maximum Value 0.23 0.55 1.6 0.02 0.01 0.8 0.35 0.02 0.004
  Component C Si Mn P S Cr Mo Ti B More
适用板厚19.1~32 Minimum Value - - - - - - - - - Ceq≤0.53
Maximum Value 0.23 0.55 1.6 0.02 0.01 0.8 0.35 0.02 0.004
  Component C Si Mn P S Cr Mo Ti B More
适用板厚32~50.8 Minimum Value - - - - - - - - - Ceq≤0.65
Maximum Value 0.23 0.55 1.6 0.02 0.01 1.2 0.5 0.02 0.004
  Component C Si Mn P S Cr Mo Ti B More
适用板厚50.9~80 Minimum Value - - - - - - - - - Ceq≤0.75
Maximum Value 0.23 0.55 1.6 0.02 0.01 1.5 0.5 0.02 0.004
EVERHARD-C450LE Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
t=5~50.8 Special Heat Treatment 450±25 -40°C
≥27
t=50.9~80 Special Heat Treatment 410~475 -40°C
≥27
t=20 Special Heat Treatment 1442 1121 19 450 -40°C
45
t=32 Special Heat Treatment 1402 1106 24 447 -40°C
33
t=50 Special Heat Treatment 1290 1008 15 469 -40°C
39