Grade SUS 304J3
Corresponding Standard JIS G 4317-2018
Hot-Formed Stainless Steel Sections
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS 304J3 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value - - - - - 17 8 1
Maximum Value 0.08 1 2 0.045 0.03 19 10.5 3
SUS 304J3 Mechanical Properties
form Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Section steel Solid Solution Treatment ≥480 ≥175 ≥40 ≤187
1 Approximate Comparison Table Austenitic Stainless Steel
China Japan International Organization for Standardization European Standard
ISC JIS ISO Numerical Grade Numerical Grade
S30480 SUS304J3 X6CrNiCu18-9-2 4567-304-98-X 1.4567
2 Approximate Comparison Table Stainless Steels for Cold Heading and Cold Extruding
China Japan International Organization for Standardization European Standard
GB ISC JIS ISO Numerical Grade EN Numerical Grade
06Cr18Ni9Cu2
(0Cr18Ni9Cu2)
S30480 SUS304J3 X6CrNiCu18-9-2 4567-304-98-X X6CrNiCu18-9-2 1.4567

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!