Grade SUS F 304H
Corresponding Standard JIS G 3214-1991
Stainless steel forgings for pressure vessels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS F 304H Chemical Element Composition Content (%)
Component C Si Mn P * S Cr Ni
Minimum Value 0.04 - - - - 18 8
Maximum Value 0.1 1 2 0.04 0.03 20 12
SUS F 304H Mechanical Properties
diameter/thickness
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
d<130 Solid Solution Treatment ≥520 ≥205 ≥43 ≥50 ≤187
130≤d≤200 Solid Solution Treatment ≥480 ≥205 ≥29 ≥45 ≤187

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!