Grade SUS F 304N
Corresponding Standard JIS G 3214-1991
Stainless steel forgings for pressure vessels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS F 304N Chemical Element Composition Content (%)
Component C Si Mn P * S Cr Ni N
Minimum Value - - - - - 18 8 0.1
Maximum Value 0.08 0.75 2 0.04 0.03 20 11 0.16
SUS F 304N Mechanical Properties
diameter/thickness
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
d<130 Solid Solution Treatment ≥550 ≥240 ≥29 ≥50 ≤217
130≤d≤200 Solid Solution Treatment ≥550 ≥240 ≥24 ≥45 ≤217