Grade SCH 12
Corresponding Standard JIS G 5122-2003
Heat-Resistant Cast Steels and Alloys for General Applications
Classification Cast Steel
Properties Corrosion Resistance
SCH 12 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.2 - - - - 18 8 -
Maximum Value 0.4 2 2 0.04 0.04 23 12 0.5
SCH 12 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
≥490 ≥235 ≥23
Approximate Comparison Table Heat-Resistant Cast Steels and Alloys
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France Russia United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST BS EN/BS
ZG25Cr18Ni9Si2 C53801 SCH 12 SCH 12
SCH 31
HRSC 12 HF J92603 GX25CrNiSi18-9 GX25CrNiSi18-9 1.4825 GX25CrNiSi18-9 10Х18Н9Л GX25CrNiSi18-9