Grade SCH 17
Corresponding Standard JIS G 5122-2003
Heat-Resistant Cast Steels and Alloys for General Applications
Classification Cast Steel
Properties Corrosion Resistance
SCH 17 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.2 - - - - 26 8 -
Maximum Value 0.5 2 2 0.04 0.04 30 11 0.5
SCH 17 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
≥540 ≥275 ≥5
1 Approximate Comparison Table Heat-Resistant Cast Steels and Alloys
Japan United States
JIS ASTM
SCH 17 HE
2 Approximate Comparison Table Heat-Resistant Cast Steels and Alloys
Japan United States Germany Russia United Kingdom
JIS ASTM UNS DIN EN/DIN W-Nr. GOST BS EN/BS
SCH13A
SCH17
HH J93503 G-X40CrNiSi25 21 1.4837 40Х24Н12Л 309C30

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!