Grade SUS315J1TP
Corresponding Standard JIS G 3459-2017(修改)
Stainless Steel Pipes (Amendment 1)
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS315J1TP Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value - 0.5 - - - 17 8.5 0.5 0.5
Maximum Value 0.08 2.5 2 0.045 0.03 20.5 11.5 3.5 1.5
SUS315J1TP Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
≥520 ≥205 ≥35