Grade SUS347TP
Corresponding Standard JIS G 3459-2017(修改)
Stainless steel pipes (Amendment 1)
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS347TP Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni More
Minimum Value - - - - - 17 9 Nb≥10C
Maximum Value 0.08 1 2 0.045 0.03 19 13
SUS347TP Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
≥520 ≥205 ≥35