Grade SUS 317
Other Names
Corresponding Standard JIS G 4305-2021
Cold-rolled stainless steel plate, sheet and strip
Brand/Supplier
Japan -> JFE Steel
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS 317 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value - - - - - 18 11 3
Maximum Value 0.08 1 2 0.045 0.03 20 15 4
①Where necessary, –CP may be attached after the above symbol of grade to indicate that the product is a plate. Example SUS 310L-CP
②Where necessary, –CS may be attached after the above symbol of grade to indicate that the product is a strip. Example SUS304-CS
SUS 317 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Solid Solution ≥520 ≥205 ≥40 ≤187
1 Approximate Comparison Table
China Taiwan, China Japan South Korea United States Germany United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
06Cr19Ni13Mo3 S31708 317 SUS 317 STS 317 317 S31700 X5CrNiMo 17-13 1.4449 317S16
2 Approximate Comparison Table
China Taiwan, China Japan South Korea United States Germany United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
06Cr19Ni13Mo3
(0Cr19Ni13Mo3)
S31708 317 SUS 317 STS 317 317 S31700 X5CrNiMo 17-13 1.4449 317S16
3 Approximate Comparison Table
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S31708 SUS317 S31700 X6CrNiMo19-13-4 4445-317-00-U (1.4445)
4 Approximate Comparison Table
China Japan United States International Organization for Standardization Russia United Kingdom
GB JIS ASTM/AISI ISO GOST BS EN/BS
0Cr19Ni13Mo3 SUS317 317 25 08X17H15M3T 317S16

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!